High Performance Solar-Blind Photodetectors Based on Plasma-Enhanced Atomic Layer Deposition of Thin Ga2O3 Films Annealed under Different Atmosphere

JOURNAL OF ALLOYS AND COMPOUNDS(2023)

Cited 16|Views11
Key words
Solar -blind photodetectors,Atomic layer deposition,Annealing