Additive Manufacturing of a High Temperature, Ni-Based Superalloy Compact Heat Exchanger: A Study on the Role of Select Key Printing Parameters
ASME JOURNAL OF HEAT AND MASS TRANSFER(2023)
Key words
laser sintering,manifold-microchannel,additive manufacturing,compact heat exchanger,Ni-based superalloys