Elaborating Strengthen Mechanism of Pt–Ir Solid Solution Superalloy at Finite Temperature

RARE METALS(2024)

Cited 7|Views28
Key words
Elastic properties,Phonon,Solid solution strengthen,Force constants,CALPHAD