Effect of Cr and Y on the Microstructure and Mechanical Properties of Fe-Cr-Al Alloys During Corrosion-Aging in Superheated Steam at 500 °C

MATERIALS CHARACTERIZATION(2024)

Cited 3|Views24
Key words
Fe-Cr-Al alloy,Phase separation,Corrosion-aging behaviors,Mechanical properties