EBSD Analysis of Grain Boundary Evolution and Dynamic Recrystallization of Inconel 625 Superalloy at Various Hot Spinning Feed Rates

Zhanjie Jing,Jiangkun Fan,Xudong Liu,Yuelin Song, Zixiao Wang,Kai Cao, Yuetan Chen, Heng Fu, Jianing Zhang,Jinshan Li

Progress in Natural Science Materials International(2024)

Cited 3|Views13
Key words
Inconel 625 superalloy,Hot spinning,Grain boundary evolution,DRX mechanism