Strain Localization in the Alloy 718 Ni-based Superalloy: from Room Temperature to 650 °C

ACTA MATERIALIA(2024)

引用 9|浏览18
关键词
Strain localization,High-resolution digital image correlation,High-temperature,Slip localization,Grain boundary sliding