Synergy Effect of Multi-Strengthening Mechanisms in CoNiCr-based High-Entropy Superalloy at Cryogenic Temperature

Yeqing Cai,Fei Liu,Yuanbiao Tan, Lixia Wang,Xuanming Ji,Song Xiang

MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING(2024)

引用 4|浏览16
关键词
High -entropy alloy,Superalloy,Cryogenic temperature,Nano -twins,Deformation mechanism