Multi-phase Material Microscopic Image Segmentation for Microstructure Analysis of Superalloys Via Modified U-Net and Rectify Strategies
COMPUTATIONAL MATERIALS SCIENCE(2024)
Key words
Multi-phase microscopic image segmentation,Superalloys,Grain boundary detection,Deep learning,Grain size,Post processing