On the Development of Equiaxed Microstructures in High-Entropy Superalloys and Their Impact on High-Temperature Oxidation Behavior

Deleted Journal(2024)

引用 0|浏览0
关键词
High-entropy superalloy,High-temperature oxidation,Microstructural characterization,Hot thermomechanical processing