Ultrathin Nanocapacitor Assembled Via Atomic Layer Deposition Javier Alonso Lopez Medina,J. Ricardo Mejia-Salazar,William O. F. Carvalho,Cesar Lopez Mercado,N. Nedev,Faustino Reyes Gomez,Osvaldo N. Oliveira Jr,M. H. Farias,Hugo TiznadoNANOTECHNOLOGY(2024)引用 0|浏览1关键词nanocapacitor,dielectric materials,atomic layer deposition,ultrathin filmsAI 理解论文溯源树样例生成溯源树,研究论文发展脉络Chat Paper正在生成论文摘要