Tracking the Onset of Plasticity in a Ni-base Superalloy Using In-Situ High-Resolution Digital Image Correlation
MATERIALS CHARACTERIZATION(2025)
Key words
Nickel alloy,Tensile,Strain localisation,Slip,EBSD,High resolution digital image correlation (HRDIC)